Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3GM35 Q643 - PA6-(GF+MD)40 - BASF

Material Data Center offers the following functions for Ultramid® B3GM35 Q643:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
--- ONLY IN THE USA AVAILABLE ---
Ultramid® B3GM35 Q643 is a combined glass-fiber and mineral reinforced injection molding PA6 grade.

Typical applications include industrial articles requiring medium rigidity and high dimensional stability.
Механические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 8100 / * МПа ISO 527
Напряжение при разрыве 117 / - МПа ISO 527
Удлинение при разрыве 2.7 / - % ISO 527
Ударная вязкость по Шарпи с надрезом, +23°C 4.1 / - кДж/м2 ISO 179/1eA
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 220 / * °C ISO 11357-1/-3
Температура изгиба под нагрузкой, 1.80 МПа 195 / * °C ISO 75-1/-2
Прочие свойствасухой / кондЕдиницаСтандарт
Водопоглощение 5.7 / * % Sim. to ISO 62
Поглощение влаги 1.7 / * % Sim. to ISO 62
Плотность 1480 / - кг/м³ ISO 1183
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 80 °C -
Время предварительной сушки 2 - 4 h -
Влажность переработки ≤0.1 % -
Температура расплава 270 - 295 °C -
Температура формы 80 - 95 °C -
Особые свойства и характеристики
Доступность материала по регионам
Другая текстовая информация
Литье под давлением
Max. Water content: 0.10%
Product is supplied in sealed containers and drying prior to molding is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 80 degC (176 degF) is recommended. Drying time is dependent on moisture level, but 2-4 hours is generally sufficient.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

Melt Temperature 270-295 degC (518-563 degF)
Mold Temperature 80-95 degC (176-203 degF)
Injection and Packing Pressure 35-125 bar (500-1500 psi)

This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics are critical, a mold surface temperature of 80-95 degC (176-203 degF) is recommended.

Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. Minimal back pressure should be utilized to
prevent glass breakage.

Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Химические вещества
Кислоты
Раствор уксусной кислоты (5% по массе) (23°C)
Раствор лимонной кислоты (10% по массе) (23°C)
Раствор молочной кислоты (10% по массе) (23°C)
Раствор соляной кислотй (36% по массе) (23°C)
Раствор азотной кислоты (40% по массе) (23°C)
Раствор серной кислоты (38% по массе) (23°C)
Раствор серной кислоты (5% по массе) (23°C)
Раствор хромовой кислоты (40% по массе) (23°C)
Щёлочи
Раствор гидроксида натрия (35% по массе) (23°C)
Раствор гидроксида натрия (1% по массе) (23°C)
Спирты
Изопропиловый спирт (23°C)
Метанол (23°C)
Этанол (23°C)
Углеводороды
н-Гексан (23°C)
Толуол (23°C)
изо-Октан (23°C)
Кетоны
Ацетон (23°C)
Простые эфиры
Диэтиловый эфир (23°C)
Минеральные масла
Всесезонное моторное масло SAE 10W40 (23°C)
Всесезонное моторное масло SAE 10W40 (130°C)
Стандартное топливо
Дизельное топливо (предпочтительно жидкость F в соотв. с ISO 1817) (23°C)
Дизельное топливо (предпочтительно жидкость F в соотв. с ISO 1817) (>90°C)
Растворы солей
Раствор хлорида натрия (10% по массе) (23°C)
Раствор гипохлорида натрия (10% по массе) (23°C)
Раствор хлорида цинка (50% по массе) (23°C)
Прочие
Этилацетат (23°C)
Перекись водорода (23°C)
Тормозная жидкость DOT 4 (130°C)
Раствор этиленгликоля в воде (50% по массе) (108°C)
Вода (23°C)
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.